Injection Molding Calculators
& Plastics Reference

Quick process checks for molders and process engineers — with the formula, the inputs and the sources on the page — plus engineering plastics data and machine alarm references.

Open Molding Tools Browse Materials Diagnose Alarms

Molding Floor Tools All tools →

Calculator

Injection Molding Clamp Tonnage Calculator

Estimate injection molding clamp force from projected area, cavities, cold runner and a tonnage factor or cavity pressure. Results in US tons,...

Calculator

Injection Molding Cooling Time Calculator

Estimate injection molding cooling time from wall thickness, thermal diffusivity and melt, mold and ejection temperatures, for flat walls or round...

Calculator

Injection Molding Residence Time & Shot Size Calculator

Estimate melt residence time and shot size as a percentage of barrel capacity from PS-rated shot capacity, resin density, shot weight and cycle...

Calculator

Resin Dryer Hopper Size & Drying Residence Calculator

Work out material throughput from shot weight and cycle time, the hopper capacity needed for your resin's drying time, and whether an existing...

Calculator

Shot Weight to Screw Stroke Calculator

Convert shot weight to injection screw stroke (and back) from screw diameter and melt density, check stroke as a multiple of screw diameter, or...

Checklists

Machine Troubleshooting by Symptom

Brand-independent checklists for heater, pressure-limit, screw recovery, clamp, ejector and hydraulic alarms.

Grade cards

Processing Conditions by Grade

Drying, barrel and mold temperatures for specific grades, taken from the supplier's own data sheet with source and revision date.

Engineering Insights View all →

Engineering Insight 2026-08-30

PEEK vs. POM (Acetal) for Gears & Bearings: A Cost-Benefit Thermoplastic Selection Guide

Comparing PEEK and POM (Acetal/Delrin) for gear and bearing applications — wear, PV limits, water absorption, dimensional stability, and when the...

Read Guide →

Engineering Insight 2026-08-30

PPS vs. PA66 for Connectors & Housings: Thermal, Moisture & Flame-Retardance Selection

Selecting between PPS and PA66 (Nylon 66) for electrical connectors, fuse boxes, and automotive housings — comparing CTI, reflow capability,...

Read Guide →

Engineering Insight 2026-08-10

Injection Molding Cost Analysis: How Material Choice Affects Part Cost

A comprehensive analysis of how material selection drives injection molding part costs, covering raw material pricing, processing premiums, cycle...

Read Guide →

Database Categories

High-Performance Polymers

74 entries

Mechanical, thermal, and processing data for engineering-grade and high-performance thermoplastics.

Machine Alarms

166 entries

Brand-specific injection molding machine alarm references and troubleshooting checks.

Material Comparisons

70 entries

Side-by-side polymer comparisons focused on application conditions, grade differences, processing, and performance trade-offs.

Engineering Thermoplastics

19 entries

Profiles for commonly specified thermoplastics, with grade and application notes where available.

Engineering Plastics Processing

5 entries

Processing references for molding, extrusion, machining, and material-specific production constraints.

compare

2 entries

Additional head-to-head polymer comparisons and material-family explainers.

High-Performance Polymers

Mechanical properties, thermal characteristics, processing guidance, and cross-referenced equivalents for engineering thermoplastics used in aerospace, medical, semiconductor, and oil & gas applications.

High-Performance Polymers

PEEK Polyetheretherketone: High-Performance Polymer Properties & Equivalents

Tensile Strength100 MPa
Melting Point343 °C
Shrinkage Rate1.2%
Flexural Modulus4.1 GPa
Hdt160 °C at 1.82 MPa
Continuous Service Temp260 °C
Tensile Modulus3.6 GPa
Yield Strength100 MPa
Elongation At Break20%
Glass Transition Temp143 °C
Compressive Strength120 MPa
Izod Impact Notched5.5 kJ/m² (high toughness)
Dielectric Strength190 kV/mm
Dielectric Constant3.3 at 1 MHz
Cte Coefficient Thermal Expansion47 µm/m-°C (below Tg)
Friction Coefficient0.20-0.35 (unfilled); 0.10 (bearing grade)
Water Absorption0.15% (24h, 23 °C)
Limiting Oxygen Index24% (inherently flame retardant)

High-Performance Polymers

Ultem PEI (Polyetherimide): High-Temperature Amorphous Thermoplastic Properties

Tensile Strength105 MPa
Melting PointN/A (Amorphous, Tg 217°C)
Shrinkage Rate0.5-0.7%
Flexural Modulus3.5 GPa
Hdt200 °C at 1.82 MPa
Continuous Service Temp170 °C
Tensile Modulus3.2 GPa
Yield Strength105 MPa
Elongation At Break10%

High-Performance Polymers

PTFE Teflon: Ultimate Chemical Resistance & Low-Friction Polymer Data

Tensile Strength25 MPa
Melting Point327 °C
Shrinkage Rate2.0-5.0%
Flexural Modulus0.6 GPa
Hdt55 °C at 1.82 MPa
Coefficient Of Friction0.04 (lowest of any solid)

High-Performance Polymers

PPS Ryton: Polyphenylene Sulfide High-Temp Chemical-Resistant Polymer

Tensile Strength90 MPa (unfilled); 160 MPa (40% GF)
Melting Point285 °C
Shrinkage Rate0.3-0.5% (40% GF)
Flexural Modulus3.8 GPa (unfilled); 14 GPa (40% GF)
Hdt265 °C at 1.82 MPa (40% GF)
Continuous Service Temp220 °C

High-Performance Polymers

LCP Vectra: Liquid Crystal Polymer for Micro-Molding & Electronic Connectors

Reference ScopePublished A130 and E130i examples, not a specification for all LCP grades
Tensile StrengthA130: 190 MPa; E130i: 150 MPa; stress at break, ISO 527-2/1A, 5 mm/min
Melting PointA130: 280°C; E130i: 335°C; 10°C/min, ISO 11357-1/-2/-3
Shrinkage RateA130: 0.2% parallel / 0.4% normal; E130i: 0.1% / 0.1%; ISO 294-4
Flexural ModulusA130: 14,500 MPa; E130i: 13,500 MPa; ISO 178, published 23°C flexural table
HdtA130: 235°C; E130i: 276°C; HDT/A at 1.8 MPa, ISO 75-1/-2
Continuous Service TempNot established for every grade or finished part by this short-term property table
Source EditionCelanese Vectra/Zenite LCP product information, LCP-026 AM 0613, p.6; historical reference, checked 2026-10-23

High-Performance Polymers

Vespel Polyimide: Extreme-Temperature Polymer for Aerospace & Semiconductor

Tensile Strength85 MPa
Melting PointN/A (Does not melt; Tg ~360°C)
Shrinkage RateN/A (Direct-formed, not molded)
Flexural Modulus3.1 GPa
Hdt360 °C
Continuous Service Temp300 °C (air); 350°C (inert)

Browse the high-performance polymer database →

Machine Alarm Diagnostics

Alarm code definitions, root cause analysis, and step-by-step troubleshooting for Netstal, Arburg, and Engel injection molding machines.

Netstal Code 102

Netstal Alarm 102: Heating Zone Temperature Out of Range - Troubleshooting Guide

SeverityHigh (Machine Stop)
ComponentHeating Band / Thermocouple
Affected SystemsInjection Unit

Arburg Code 320

Arburg Error 320: Barrel Heating Control Failure - Troubleshooting Guide

SeverityCritical (Interlock)
ComponentSolid State Relay / Heating Circuit
Affected SystemsHeating Controller / Selogica

Engel Code 405

Engel Alarm 405: Screw Recovery Time Exceeded - Diagnostics & Fix

SeverityMedium (Cycle Delay / Warning)
ComponentScrew Drive Motor / Hydraulic Pump
Affected SystemsPlasticizing Unit / CC300 Controller

Netstal Code 301

Netstal Alarm 301: Mold Protection Force Exceeded - Troubleshooting

SeverityCritical (Immediate Stop)
ComponentMold Protection System / Clamping Unit
Affected SystemsClamp / Mold Safety

Sumitomo Demag Code 220

Sumitomo Demag Alarm 220: Clamp Force Not Reached - Diagnostics & Troubleshooting

SeverityHigh (Cycle Interruption)
ComponentClamping Unit / Hydraulic System
Affected SystemsClamp Cylinder / NC5 Controller

KraussMaffei Code MC45

KraussMaffei Alarm MC45: Injection Pressure Limit Exceeded - Troubleshooting Guide

SeverityHigh (Process Deviation / Cycle Stop)
ComponentInjection Unit / Hydraulic System
Affected SystemsMC6 Controller / Injection Cylinder

View all 166 alarm entries →

Material Comparisons

Side-by-side selection guides comparing high-performance polymers across mechanical, thermal, chemical, and cost dimensions. Designed for materials engineers making critical polymer decisions.

Comparison

PEEK vs Ultem PEI: Which High-Performance Polymer Should You Choose?

MaterialsPEEK (Polyetheretherketone) vs Ultem PEI (Polyetherimide)
Key Differentiator
CostPEEK 2-3× more expensive than Ultem PEI

Comparison

PPS Ryton vs LCP Vectra: Which Ultra-Flow High-Temp Polymer for Precision Parts?

MaterialsPPS Ryton (Polyphenylene Sulfide) vs LCP Vectra (Liquid Crystal Polymer)
Key Differentiator
CostPPS is 50-70% of LCP cost

Comparison

PTFE Teflon vs PEEK: Chemical Resistance vs Mechanical Strength Trade-Off

MaterialsPTFE Teflon (Polytetrafluoroethylene) vs PEEK (Polyetheretherketone)
Key Differentiator
CostPTFE is 30-50% of PEEK cost

Comparison

Vespel Polyimide vs PEEK: When the Highest-Temperature Polymer Is the Only Option

MaterialsVespel PI (Polyimide) vs PEEK (Polyetheretherketone)
Key Differentiator
CostVespel SP-1 5-10× more expensive than PEEK

Comparison

Torlon PAI vs Vespel PI: Ultimate High-Temperature Polymer Comparison

MaterialsTorlon PAI (Polyamide-imide) vs Vespel PI (Polyimide)
Key DifferentiatorTorlon: lower cost, easier processing. Vespel: 100°C higher continuous service.
CostTorlon: $$ | Vespel: $$$$

Comparison

Glass Fiber vs Carbon Fiber Reinforced Thermoplastics: Complete Performance Comparison

MaterialsGlass Fiber Reinforced (GFR) Thermoplastics vs Carbon Fiber Reinforced (CFR) Thermoplastics
Key DifferentiatorCFR provides 2-3× higher stiffness-to-weight ratio and electrical conductivity vs GFR's lower cost and radio-transparency
Cost

View all 72 comparison guides →

Recently Added

Why Propprose?

Source-Aware

Material and alarm references point to source documents where available. Verify the exact grade, test conditions, and machine revision before making a design or maintenance decision.

Zero Latency

Pre-built static pages served via CDN. No database queries, no API calls — instant page loads worldwide.

B2B Focused

Built for manufacturing engineers, process technicians, and procurement specialists — not hobbyists.